Nguzogide corrosion nke R-SiC na Si3N4-SiC na Aluminom-silicon Alloy Melt

Silicon carbide na silicon nitride nwere adịghị mma wettability na ọla a wụrụ awụ. E wezụga ịbụ infiltrated site magnesium, nickel, chromium alloy na igwe anaghị agba nchara, ha enweghị wettability na ndị ọzọ ọla, n'ihi ya, ha nwere magburu onwe corrosion iguzogide na-eji ọtụtụ ebe na aluminum electrolysis ụlọ ọrụ.

N'ime akwụkwọ a, a na-enyocha nguzogide corrosion nke silicon carbide R-SiC na silicon nitride bonded silicon carbide Si3N4-SiC na Al-Si alloy na-ekpo ọkụ na-agbaze site na ọtụtụ latitudes.

Dị ka nnwale data nke 9 ugboro nke thermal ịgba ígwè nke 1080h na 495 Celsius C ~ 620 Celsius C aluminum-silicon alloy gbazee, na-esonụ analysis results nwetara.

Ihe nlele R-SiC na Si3N4-SiC mụbara na oge nrụrụ na ọnụ ọgụgụ corrosion belatara. Ọnụego corrosion dabara na mmekọrịta logarithmic nke attenuation. (nọmba nke 1)

ịrụ ọrụ nguzogide iyi (1)

Site na nyocha ike dị iche iche, ihe nlele R-SiC na Si3N4-SiC n'onwe ha enweghị aluminom-silicon; na ụkpụrụ XRD, ụfọdụ ego nke aluminom-silicon elu bụ elu-ihe fọdụrụ aluminom-silicon alloy. (Foto nke 2 - foto 5)

Site na nyocha SEM, ka oge mmebi ahụ na-abawanye, usoro nhazi nke R-SiC na Si3N4-SiC dị nro, ma ọ dịghị mmebi doro anya. (Foto nke 6 - foto 7)

ịrụ ọrụ nguzogide iyi (2)

Esemokwu dị n'elu σs / l> σs / g nke interface n'etiti mmiri mmiri aluminom na seramiiki, akụkụ wetting θ n'etiti oghere dị> 90 Celsius, na interface n'etiti mmiri mmiri aluminom na mpempe akwụkwọ seramiiki adịghị mmiri.

Ya mere, ihe R-SiC na Si3N4-SiC dị mma na nguzogide corrosion megide aluminum silicon gbazee ma nwee obere ọdịiche. Agbanyeghị, ọnụ ahịa ihe Si3N4-SiC dị obere ma etinyere ya nke ọma kemgbe ọtụtụ afọ.